In this study, tensile tests of 63Sn/37Pb solder were carried out at various strain rates from 10−5 s−1 to 10−1 s−1 over a wide temperature range from −40°C to 125°C to study the effect of strain rate and testing temperature on the mechanical properties in a systematic manner. Based on these experimental data, a set of empirical formulae was derived by a statistical method to describe the effect of temperature and strain rate in a quantitative manner and explain the variation in the mechanical properties published in other reports. It is concluded that the empirical formulae can be used to characterize the mechanical properties of 63Sn/37Pb over a wide range of temperatures and strain rates.
Issue Section:
Technical Papers
1.
Furukawa
M.
Ma
Y.
Horita
Z.
Nemoto
M.
Valley
R. Z.
Langdon
T. G.
1998
, “Microstructural Characteristics and Superplastic Ductility in A Zn-22% Al Alloy with Submicrometer Grain Size
,” Materials Science and Engineering
, Vol. A241
, pp. 122
–128
.2.
Han
B. Q.
Chan
K. C.
1997
, “High-Strain-Rate Superplasticity of An AL2009-SICw Composite
,” Journal of Materials Science Letters
, Vol. 16
, pp. 827
–829
.3.
JEDEC (Joint Electronic Device Engineering Council) Standard, 1989, “Temperature Cycling,” JESD22-A104-A, Electronic Industries Association, USA.
4.
JEDEC (Joint Electronic Device Engineering Council) Standard, 1995, “Thermal Shock,” JESD22-A106-A, Electronic Industries Association, USA.
5.
Jones, W. K., Liu, Y. Q., Zampino, M. A., and Gonzalez, G. L., 1997, “The At-Temperature Mechanical Properties of Lead-Tin Based Alloys,” Advancing Microelectronics, pp. 30–34.
6.
Kilinski, T. J., Lesniak, J. R., and Sandor, B. L, 1991, “Modern Approaches to Fatigue Life Prediction of SMT Solder Joints,” Solder Joint Reliability: Theory and Applications, J. Lau, ed., pp. 384–390.
7.
Kondo
T.
Takigawa
Y.
Sakuma
T.
1997
, “High-Temperature Tensile Ductility in TZP and TiO2—Doped TZP
,” Materials Science and Engineering
, Vol. A231
, pp. 163
–169
.8.
Lau, J., and Pao, Y. H., 1997, Solder Joint Reliability of BGA, Flip Chip, CSP, and Fine Pitch SMT Assemblies, Van Nostrand Reinhold, New York.
9.
Li
M. Q.
Chen
Y.
1997
, “Superplastic Deformation of SiCp/2024 A1 Composite Fabricated by Spray Atomization and Codeposition
,” Journal of Materials Engineering and Performance
, Vol. 6
(5
), pp. 664
–666
.10.
Liu, S., and Qing, Z. F., 1997, “A Unified Viscoplastic Constitutive Model for Tin-Lead Solder Joints,” Advances in Electronic Packaging, ASME EEP-Vol. 19-2, pp. 1599–1604.
11.
Ninomiya, R., and Miyake, K., 1997, “Microstructure and Mechanical Properties of New Lead-Free Solder,” Advances in Electronic Packaging, pp. 1329–1333.
12.
Sandor
B. I.
Ju
S. H.
Plesha
M. E.
1996
, “Life Prediction of Solder Joints by Damage and Fracture Mechanics
,” ASME JOURNAL OF ELECTRONIC PACKAGING
, Vol. 118
, pp. 193
–200
.13.
Skipor
A. F.
Harren
S. V.
Botsis
J.
1996
, “On the Constitutive Response of 63/37 Sn/Pb Eutectic Solder
,” ASME Journal of Engineering Materials and Technology
, Vol. 118
, pp. 1
–11
.14.
Vaynman, S., and Fine, M. E., 1989, “Fatigue of Low-Tin Lead-Based and Tin-Lead Eutectic Solders,” Microelectronic Packaging Technology, W. T. Shieh, ed., pp. 255–259.
This content is only available via PDF.
Copyright © 1999
by The American Society of Mechanical Engineers
You do not currently have access to this content.